White ink on a black t-shirt is one of the most requested prints, and it is also the one that gives beginners the most trouble. You print, you lift the screen, and the white has turned grey, or you can see the weave of the fabric through the design. It is rarely the "wrong" ink: almost always the cause is the thickness of the ink layer, the screen and how you dry between one pass and the next.
In this guide you will find what you need, which white to choose between water-based and plastisol, and the step-by-step process for a solid white on black, even with a DIY setup.
Why white on black is harder
On a white t-shirt the ink only has to add colour. On a black t-shirt it has to cover the colour underneath. Cotton absorbs part of the ink, so if the layer is thin the black fabric shows through and the white looks dull.
That is why printing on dark shirts needs three things together: an opaque white ink, a screen that lets enough ink through and, in most cases, two passes with a drying step in between.
What you need
- A 55T screen. The number tells you how many threads there are in one centimetre of mesh: fewer threads means more open mesh and more ink on the shirt. 55T is the most used screen for t-shirts and the right one for white on black.
- An opaque white ink, water-based or plastisol (see below).
- A water-resistant photo emulsion if you use water-based inks: an emulsion that is not made for them would break down during printing.
- A squeegee and a rigid surface where the t-shirt stays flat and tight.
- A heat source to dry between passes and for final curing: a heat gun, a heat press or a screen printing dryer.
Water-based or plastisol: which white to choose
Both cover on black, but you work them differently.
Water-based white ink
The ACRILTEX white water-based screen printing ink covers well on black and dark t-shirts, gives a soft print that moves with the fabric and cleans up with water. It works on cotton, blends and also on polyester and polyamide.
- It air-dries in 20-30 minutes.
- It is heat cured at 90 °C: 3-4 minutes in a screen printing dryer, 5-20 seconds with a heat press, or with an iron, placing a sheet of silicone or baking paper between the iron and the shirt.
- You can thin it with up to 5% water, but white should be thinned as little as possible: the thinner it is, the less it covers.
Watch the screen: water-based ink can dry in the mesh if you leave it sitting. Print without long breaks and wash the screen right after printing.
White plastisol ink
The white plastisol screen printing ink is made for high opacity on light and dark fabrics. It does not air-dry: it stays workable in the screen until you heat it.
- Between passes it gels (flash) in a few seconds at 130-150 °C.
- Final curing, according to the technical data sheet, is 150 °C for 2-3 minutes, or 130-150 °C for 3-5 minutes.
- For maximum coverage on dark fabrics the data sheet recommends 43-55 threads/cm mesh.
In short: if you print a few shirts and want to clean everything with water, start with water-based. If you want the most solid white and plan longer runs, plastisol is easier because it does not dry in the screen.
Step by step: white on a black t-shirt
- Prepare the 55T screen. Degrease the mesh, coat it with emulsion, let it dry in the dark and expose your design as usual.
- Fix the t-shirt. It must lie flat and still on the platen. Put a piece of card inside so the ink does not go through to the back.
- Fix the screen. To print twice in the same spot, the screen has to come back exactly where it was. Hinge clamps already do a good job; with a screen printing press the screen always stays in the same position.
- First pass. Load plenty of ink above the design and pull the squeegee with firm, even pressure at about 45°.
- Flash without moving the shirt. Lift the screen and pass the heat gun over the print, always moving and a few centimetres away, until the layer is dry to the touch (water-based) or gelled (plastisol). Do not stay on one spot: the fabric can scorch.
- Second pass. Lower the screen and print again. The second layer sits on the first and the white becomes solid.
- Final cure. Cure the print at the times and temperatures above for the ink you are using. The heat gun is for drying between passes: with plastisol it does not replace a dryer or a heat press for the final cure.
Common mistakes
- The white comes out grey: the layer is too thin. Check you are using a 55T screen, do not over-thin the ink and do the second pass.
- The edges spread: the screen or the shirt moved between the two passes, or there was too much ink under the screen. Fix both more firmly.
- The ink dries in the screen: it happens with water-based ink during long breaks or in hot weather. Print without stopping and clean the screen as soon as you finish.
- The print is damaged after the first wash: it was not cured enough. Follow the times and temperatures on the ink data sheet.
Where to start
If you want to start printing white on black, the T-Shirt Screen Printing Starter Kit already includes the 55T screen, the emulsion, the LED UV lamp to expose the screen, the squeegee and the ink: when you order, you can choose white ink instead of black. Add the heat gun to dry between passes.
If you plan to print regularly, the T-Shirt Screen Printing Kit with the K-SER Zero press keeps the screen always in the same position: that is what matters most when you have to print twice in the same spot, shirt after shirt.
FAQ
How many passes do I need for white on black?
Usually two, with a flash in between. With one pass the white tends to stay grey, especially with water-based inks.
Can I cure white ink with an iron?
With the ACRILTEX white water-based ink, yes: at 90 °C, with a sheet of silicone or baking paper between the iron and the shirt. For plastisol follow the temperatures in the data sheet, with a heat press or a dryer.
Which screen should I use for white on black?
A 55T screen, which lays down a thicker layer. 77T works for designs with many fine details, but it covers less.
Leave a Comment